Researchers in Korea have been developing improved non-alloyed contacts for gallium arsenide (GaAs) complementary metal-oxide-semiconductor (CMOS) and high-electron-mobility transistors (HEMTs) [Seung-Hwan Kim et al, IEEE Electron Device ...
SAMCO Inc of Kyoto, Japan, a supplier of plasma etch, chemical vapour deposition (CVD) and surface treatment systems to compound semiconductors device makers, has launched an atomic layer deposition (ALD) system focusing on gate oxide ...
Ultratech, a supplier of lithography, laser--processing and inspection systems used to manufacture semiconductor devices and high-brightness LEDs (HBLEDs), as well as atomic layer deposition (ALD) systems, today announced that it has ...
Tags: Wafer-Level Packaging, LEDs
Researchers in the USA and Korea have developed a hydrogen high pressure annealing (HPA) process for aluminium oxide/hafnium dioxide (Al2O3/HfO2) gate stacks on indium gallium arsenide (InGaAs) quantum wells [Tae-Woo Kim et al, IEEE ...
Tags: Transistors, capacitors
Researchers in China and Hong Kong have claimed the highest output power density and power-added efficiency reported to date for gallium nitride (GaN)-based enhancement-mode metal-insulator-semiconductor high-electron-mobility transistors ...
Tags: GaN MIS-HEMTs, PECVD ALD MOCVD
CVD Equipment Corp of Central Islip, NY, USA (a designer and maker of equipment for developing and manufacturing electronic components, materials and coatings for research and industrial applications) is entering into an industrial ...
Tags: CVD Equipment, 2D materials
Epitaxial deposition and process equipment maker Veeco Instruments Inc of Plainview, NY, USA has reported revenue for full-year 2014 of $392.9m, up 18% on $331.7m in 2013. Fourth-quarter 2014 revenue was $113.6m, up 22% on $93.3m last ...
RASIRC Inc of San Diego, CA, USA, whose products purify and deliver ultra-pure liquids and gases, has announced independent test results by the University of California, San Diego (UCSD) that show high-purity hydrogen peroxide vapor ...
Tags: RASIRC, ultra-pure liquids
In Kolkata and Delhi, Oxford Instruments is hosting its third series of annual seminars for the nanotechnology industry in India. ‘Bringing the Nanoworld Together 2014’ will showcase nanotechnology tools and their use in ...
Tags: Oxford Instruments, Seminars, Electronics
Riber S.A. of Bezons, France, which manufactures molecular beam epitaxy (MBE) systems as well as evaporation sources and effusion cells, has signed a distribution agreement with AnnealSys SAS of Montpellier, France, which specializes in ...
Tags: Riber, MBE systems
Agnitron Technology Inc of Eden Prairie, MN, USA is scheduled to ship its latest 1500°C+ reactor upgrade for the Veeco metal-organic chemical vapor deposition (MOCVD) D-series Legacy System platform. The single 2”- or ...
Tags: Veeco MOCVD, Reactor
Researchers in Taiwan have applied a non-vacuum process to deposit aluminium oxide (Al2O3) passivation for nitride semiconductor high-electron-mobility transistors (HEMTs) [Bo-Yi Chou et al, IEEE Electron Device Letters, published online 11 ...
Tags: Electrical, Electronics, Transistor
Turkey's Bilkent University has used hollow-cathode plasma-assisted atomic layer deposition (HCPA-ALD) to make gallium nitride (GaN) thin-film transistors (TFTs) at temperatures below 250°C [S. Bolat et al, Appl. Phys. Lett., vol104, ...
Tags: HCPA-ALD GaN Thin-film transistors, Electrical, Electronics, Transistors
Researchers based in USA and South Korea have developed a gate stack for III-V quantum well metal-oxide-semiconductor field-effect transistors (QW MOSFETs) based on a bilayer dielectric of beryllium oxide (BeO) and hafnium dioxide (HfO2) ...
Tags: InGaAs MOSFETs QW MOSFETs InGaAs ALD, Electrical, Electronics
For first quarter 2014, epitaxial deposition and process equipment maker Veeco Instruments Inc of Plainview, NY, USA has reported revenue of $90.8m, up 24% on $73.2m last quarter and 47% on $61.8m a year ago. Growth was driven mainly by ...
Tags: Veeco, LED backlighting